Title Multilayered vacuum-arc nanocomposite TiN/ZrN coatings before and after annealing: Structure, properties, first-principles calculations
Authors Pohrebniak, Oleksandr Dmytrovych  
Bondar, Oleksandr Viacheslavovych  
Postolnyi, Bohdan Oleksandrovych
Ivashchenko, V.I.
Beresnev, V.M.
Sobol, O.
Załęski, K.
Jurga, S.
Coy, E.
Konarski, P.
ORCID http://orcid.org/0000-0002-9218-6492
http://orcid.org/0000-0003-3174-0709
Keywords TiN/ZrN
Multilayers
Hardness
Nanoscale
Nanocrystals
First-principles calculations
Type Article
Date of Issue 2017
URI http://essuir.sumdu.edu.ua/handle/123456789/64236
Publisher Elsevier
License
Citation Multilayered vacuum-arc nanocomposite TiN/ZrN coatings before and after annealing: Structure, properties, first-principles calculations [Текст] / A. Pogrebnjak, V. Ivashchenko, O. Bondar [et al.] // Materials Characterization. — 2017. — №134. — P. 55-63.
Abstract Nanoscale multilayered TiN/ZrN films were deposited using sequential vacuum-arc deposition of Ti and Zr targets in a nitrogen atmosphere. Studies of film's properties were carried out using various modern methods of analysis, such as XRD, STEM, HRTEM, SIMS combined with results of nanoindentation and tribological tests. To interpret the mechanical properties of the deposited multilayer films first-principles calculations of TiN(111), ZrN(111) structures and TiN(111)/ZrN(111) multilayer were carried out. To study the influence of thermal annealing, several samples were annealed in air at the temperature 700 °C. All deposited samples were highly polycrystalline with quite large 20–25 nm crystals. The crystalline planes were very ordinated and demonstrated an excellent coordinated growth. The nanohardness and elastic modulus of non-annealed coatings reached 42 GPa and 348 GPa, respectively. Annealing in air at the temperature 700 °C led to partial oxidation of the multilayered coatings, however hardness of the non-oxidized part of the coatings remained as high, as for initial coatings. All deposited coatings demonstrate good wear resistance.
Appears in Collections: Наукові видання (ЕлІТ)

Views

Canada Canada
1
Finland Finland
1
Germany Germany
23244248
Greece Greece
1
Ireland Ireland
787624
Lithuania Lithuania
1
Netherlands Netherlands
15097
Russia Russia
2
Sweden Sweden
1
Ukraine Ukraine
196869360
United Kingdom United Kingdom
99669552
United States United States
1749454654
Unknown Country Unknown Country
196869358
Vietnam Vietnam
73183

Downloads

Australia Australia
11622679
Belgium Belgium
1
China China
-2027984209
France France
1
Germany Germany
61456901
Hong Kong SAR China Hong Kong SAR China
73178
India India
23244255
Iran Iran
61456901
Ireland Ireland
4924390
Israel Israel
1
Japan Japan
1
Lithuania Lithuania
1
Nigeria Nigeria
1
Poland Poland
-2027984212
Romania Romania
1
South Korea South Korea
1
Taiwan Taiwan
1
Thailand Thailand
1
Turkey Turkey
1
Ukraine Ukraine
714397789
United Kingdom United Kingdom
1
United States United States
-2027984212
Unknown Country Unknown Country
120
Vietnam Vietnam
253238

Files

File Size Format Downloads
Pogrebnjak_Multilayered_vacuum.pdf 1,52 MB Adobe PDF -911555874

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.