Please use this identifier to cite or link to this item: https://essuir.sumdu.edu.ua/handle/123456789/81811
Or use following links to share this resource in social networks: Recommend this item
Title Microstructure and tribomechanical properties of multilayer TiZrN/TiSiN composite coatings with nanoscale architecture by cathodic-arc evaporation
Authors Maksakova, Olga Vasylivna
Kravchenko, Yaroslav Olehovych  
Pogrebnjak, Oleksandr Dmytrovych
Zhanyssov, S.
ORCID http://orcid.org/0000-0003-0984-1298
Keywords
Type Article
Date of Issue 2020
URI https://essuir.sumdu.edu.ua/handle/123456789/81811
Publisher springer
License Copyright not evaluated
Citation Maksakova, O.V., Zhanyssov, S., Plotnikov, S.V. et al. Microstructure and tribomechanical properties of multilayer TiZrN/TiSiN composite coatings with nanoscale architecture by cathodic-arc evaporation. J Mater Sci 56, 5067–5081 (2021). https://doi.org/10.1007/s10853-020-05606-2
Abstract Multilayer TiZrN/TiSiN coatings were deposited on steel substrate by the cathodicarc evaporation technique. The TiZr (75:25 at. %) and TiSi (95:5 at. %) alloy cathodes served as evaporation sources. Scanning electron microscopy with energy-dispersive spectroscopy, secondary ion mass-spectrometry, X-ray diffraction and X-ray photoelectron spectroscopy were employed to investigate the microstructure, elemental composition, phase state and bonding structure of the deposited coatings. Nanoindentation and ball-on-disk tribology tests were used tomeasure themechanical and tribological features of the coatings, such as hardness, elastic modulus, toughness, friction coefficient and wear rate. The results show that all multilayers were fcc structureswith a strong preferred orientation along (111) plane. The coherent growth of the multilayers contributed to the formation of the fine-grained structure with crystallites of 9.2–11.6 nm size and a lowlevel of residual stresses of- (3.5–5.3) GPa. All multilayer coatings exhibited high hardness up to 38.2 ± 1.15 GPa and elastic modulus up to 430 ± 12.9 GPa, indicating higher resistance against plastic deformation compared to TiZrN and TiSiN films. The result of ball-on-disk wear tests showed that the multilayer sample with the best structural features (modulation period of 20.4 nm, 0.86 at. % of Si, the crystallite size of 9.2 nm and residual stress of- 3.5 GPa)demonstrated the lowest friction coefficient of 0.844 andbetterwear rate of 3.32 10–5 mm3/N m.
Appears in Collections: Наукові видання (ЕлІТ)

Views

China China
29193712
Finland Finland
1
Germany Germany
1
Greece Greece
1
Ireland Ireland
45077
Lithuania Lithuania
1
Netherlands Netherlands
289
Singapore Singapore
1
Sweden Sweden
23212
Ukraine Ukraine
3828176
United Kingdom United Kingdom
1314878
United States United States
22852327
Unknown Country Unknown Country
1
Uzbekistan Uzbekistan
1
Vietnam Vietnam
2708

Downloads

Algeria Algeria
1
Canada Canada
1
China China
29193712
Germany Germany
1314875
India India
9864
Ireland Ireland
116455
Italy Italy
1
Kazakhstan Kazakhstan
1
Lithuania Lithuania
1
Malaysia Malaysia
1
Mexico Mexico
1
Poland Poland
29193713
Portugal Portugal
1
South Africa South Africa
1
South Korea South Korea
1
Taiwan Taiwan
1314880
Ukraine Ukraine
10169557
United Kingdom United Kingdom
116455
United States United States
22852328
Vietnam Vietnam
1

Files

File Size Format Downloads
Maksakova Microstructure.pdf 218,32 kB Adobe PDF 94281850

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.