Please use this identifier to cite or link to this item: https://essuir.sumdu.edu.ua/handle/123456789/90406
Or use following links to share this resource in social networks: Recommend this item
Title Photoluminescence and Thermoluminescence Studies of Dysprosium (Dy3+) Doped Zinc Aluminate Nanophosphor (Zn0.97Al2O4:0.03Dy)
Other Titles Дослідження фотолюмінесценції та термолюмінесценції нанолюмінофору алюмінату цинку, легованого диспрозієм (Dy3+) (Zn0.97Al2O4:0.03Dy)
Authors Pankaj, Pathak
Manisha, Singh
Pankaj, Kumar Mishra
Ranjeet, Brajpuriya
ORCID
Keywords нанолюмінофори
люмінесценція
алюмінати
XRD
FTIR
LED
пасивний дозиметр
nanophosphors
luminescence
aluminates
passive dosimeter
Type Article
Date of Issue 2022
URI https://essuir.sumdu.edu.ua/handle/123456789/90406
Publisher Sumy State University
License In Copyright
Citation Pankaj Pathak, Manisha Singh, et al., J. Nano- Electron. Phys. 14 No 6, 06019 (2022) DOI: https://doi.org/10.21272/jnep.14(6).06019
Abstract У статті ми повідомляємо про алюмінат цинку (ZnAl2O4), легований нанолюмінофором з 0,03 моль % диспрозію (Dy3+), із загальною формулою Zn(1 – x)Al2O4:x(x = 0.03 mol. %)Dy завдяки його люмінесцентним властивостям та різним застосування. З використанням сечовини як палива методом спалювання отримано нанолюмінофор ZnAl2O4, легований диспрозієм (Dy3+). Синтезовані нанолюмінофори були охарактеризовані за допомогою XRD, TEM, SEM з EDS та FTIR спектроскопією. За результатами XRD досліджень було встановлено, що середній розмір кристалітів становить 18,10 нм з просторовою групою Fd3ˉm і параметрами решітки a = b = c ~ 8.100 Å. Електронна дифракція вибраної області (SAED) виявила концентричні кола, зумовлені полікристалічністю. Два піки при 652,10 см – 1 і 545,19 см – 1, які спостерігаються за допомогою FTIR спектроскопії, відповідають алюмінату (AlO6), що вказує на утворення нанолюмінофора Zn0.97Al2O4:0.03Dy. Для дослідження фотолюмінісцентних (PL) властивостей використовувалася лампа Xe з довжиною хвилі 360 нм як джерело збудження. Спектри збудження та випромінювання оцінювали в діапазоні від 200 до 400 нм та від 400 до 600 нм відповідно. Пік збудження спостерігався при 305 нм. Для довжини хвилі збудження (λex = 305 нм) спектри випромінювання записували при 476 нм і 574 нм. Для дослідження термолюмінесценції (TL) зразок був попередньо опромінений рентгенівським випромінюванням високої енергії з дозою в діапазоні від 500 до 1000 Gy. Кінетичні параметри, такі як енергія активації та частотний фактор, були розраховані за кривою світіння TL. Результати показують, що Zn0.97Al2O4:0.03Dy може бути потенційно використаний як синій випромінюючий діод та пасивний дозиметр з високою радіацією.
In the present paper, we have reported zinc aluminate (ZnAl2O4) doped with 0.03 mol. % of dysprosium (Dy3+) nanophosphor with general formula Zn(1 – x)Al2O4:x(x = 0.03 mol. %)Dy for its luminescence properties and applications. Using urea as fuel, ZnAl2O4 doped with dysprosium (Dy3+) nanophosphor was prepared by the combustion method. The synthesized nanophosphors were characterized with XRD, TEM, SEM with EDS and FTIR spectroscopy. From XRD studies, the average crystallite size was found to be 18.10 nm with space group Fd3 – m and lattice parameters a = b = c ~ 8.100 Å. The selected area electron diffraction (SAED) revealed concentric circles which are due to polycrystallinity. The two peaks at 652.10 cm – 1 and 545.19 cm – 1 observed in FTIR spectroscopy correspond to aluminate (AlO6), which indicates the formation of Zn0.97Al2O4:0.03Dy nanophosphor. For photoluminescence (PL) properties, a Xe lamp with 360 nm wavelength was utilized as an excitation source for the measurement. The excitation and emission spectra were evaluated in the range of 200 to 400 nm and 400 to 600 nm, respectively. An excitation peak at 305 nm was observed. For the excitation wavelength (λex = 305 nm), emission spectra were recorded at 476 nm and 574 nm. For thermoluminescence (TL), the sample was pre-irradiated with high energy X-rays under Elekta Synergy radiation generating machine with a dose ranging from 500-1000 Gy. The kinetic parameters like activation energy and frequency factor were calculated from the TL glow curve. The results indicate that Zn0.97Al2O4:0.03Dy could be a potential candidate as a blue-emitting diode and a high radiation passive dosimeter.
Appears in Collections: Журнал нано- та електронної фізики (Journal of nano- and electronic physics)

Views

China China
1
Germany Germany
3823
India India
171291
Ireland Ireland
1
Mexico Mexico
1
Netherlands Netherlands
1
Pakistan Pakistan
68
Tunisia Tunisia
1
Ukraine Ukraine
1261580
United Kingdom United Kingdom
11672
United States United States
2741215
Unknown Country Unknown Country
31196

Downloads

China China
11671
India India
171292
Japan Japan
1
Pakistan Pakistan
2395
South Korea South Korea
1
Ukraine Ukraine
1261581
United States United States
825466
Unknown Country Unknown Country
976

Files

File Size Format Downloads
Pankaj_Pathak_jnep_6_2022.pdf 733,36 kB Adobe PDF 2273383

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.